Abstract
An approximately 1.5 μm-thick Al film was first deposited on the AlN surface by radio-frequency magnetron sputtering, followed by vacuum brazing of the AlN ceramic to an Al substrate using an Al–10.5Si–1.5 Mg(wt.%) filler metal. Brazing was conducted at 550–590 °C for 20 min to investigate the effects of brazing temperature on the joint microstructure, mechanical properties. During cooling, the preferential growth of α-Al rejected Si into the residual liquid, resulting in local Si enrichment within the brazing seam. Among the investigated conditions, the joint brazed at 580 °C exhibited the most uniform brazing seam and achieved the highest shear strength of 55 ± 2 MPa. The 580 °C joint exhibited an effective thermal conductivity of 196.3 W m−1 K−1 at 25 °C. These results demonstrate the feasibility of low-temperature AlN/Al joining using Al metallization and Al–Si–Mg filler metal, with potential applications in electronic thermal-management components.
| Original language | English |
|---|---|
| Journal | Ceramics International |
| DOIs | |
| Publication status | Accepted/In press - 2026 |
| Externally published | Yes |
Keywords
- AlN/Al joints
- Al–Si–Mg filler metal
- Magnetron sputtering
- Thermal conductivity
- Vacuum brazing
Fingerprint
Dive into the research topics of 'Microstructure and mechanical properties of AlN/Al joints vacuum brazed with Al–Si–Mg filler metal'. Together they form a unique fingerprint.Cite this
- APA
- Author
- BIBTEX
- Harvard
- Standard
- RIS
- Vancouver