Abstract
The microstructure and the mechanical properties of TiB2 ceramics synthesized by the spark plasma sintering (SPS) process with Ti sinter-aid were investigated. The results indicate that the addition of 2.5 wt.% Ti significantly decreases the densification temperature of the TiB2 ceramic. The TiB2 ceramic sintered at 1650 °C exhibits the highest relative density of 99.1%, a microhardness of 26.8 ± 1.6 GPa, a flexural strength of 558 ± 39 MPa and a fracture toughness of 5.9 ± 0.3 MPa m1/2.
| Original language | English |
|---|---|
| Pages (from-to) | 167-170 |
| Number of pages | 4 |
| Journal | Scripta Materialia |
| Volume | 66 |
| Issue number | 3-4 |
| DOIs | |
| Publication status | Published - Feb 2012 |
Keywords
- Grain growth
- Mechanical properties
- Microstructure
- Sintering
- Titanium diboride