Integrating Atomistic Simulations and Experimental Techniques to Unveil Hydrogen Trapping in Metal Carbide-Strengthened α-Fe

  • Fatima Shehzadi
  • , Yangwei Wang*
  • , Saeed Jamal
  • , Lintao Gui*
  • , Jian Wang
  • , Mirza Muhammad Abu Bakar Baig
  • , Tahir Mehmood Bhatti
  • , Irfan Ali Abro
  • , Yan Zhao*
  • *Corresponding author for this work
  • Beijing Institute of Technology
  • Ltd.

Research output: Contribution to journal › Article › peer-review

Abstract

Hydrogen embrittlement (HE) remains a critical challenge in the development of ultra-high strength steels for demanding applications such as automotive safety components. The present study explores the comparative efficacy of niobium carbides (NbC) and vanadium carbides (VC) precipitates in trapping hydrogen and mitigating HE in novel press hardened steel 34MnB5Nb compared with 34MnB5V by experimental and first principles computational approaches. The NbC exhibits superior resistance to HE, demonstrated by a lower total elongation loss (27.2%) compared to the VC counterpart (32.6%) under hydrogen charged conditions. TDS analysis revealed stronger irreversible hydrogen trapping in NbC, evidenced by a dominant second desorption peak at 450 °C and a unique third peak at 650–700 °C. Microstructural characterization confirmed finer and more uniformly distributed NbC precipitates (~ 26 nm) than VC (~ 41 nm), enhancing hydrogen immobilization. First principles density functional theory (DFT) calculations revealed that NbC exhibits a higher hydrogen trapping energy (−5.71 eV vs. −5.67 eV for VC), stronger charge localization at carbon vacancy sites and more pronounced d-state hybridization near the Fermi level. Charge density distribution maps showed enhanced electron confinement around hydrogen in NbC as compared to VC, while Bader charge analysis confirmed greater charge transfer stability. Furthermore, NbC/α-Fe interfaces demonstrated higher strain energy (5.81 eV) than VC/α-Fe (−0.27 eV), suppressing coarsening and maintaining fine precipitate dispersion. The findings confirm that NbC offers more efficient and stable hydrogen trapping, making it superior for improving hydrogen tolerance in advanced high-strength steels. Geometric Phase Analysis (GPA) showed that NbC precipitates produce sharply localized interfacial strain, whereas VC displays a more diffuse distortion pattern, consistent with the calculated carbide/Fe lattice misfit (≈ 21–27%) and indicating distinct strain-driven trapping environments arising from both vacancy-mediated bulk trapping and interface-mediated trapping mechanisms. The NEB calculations further show that NbC presents a higher hydrogen diffusion barrier (0.68 eV) than VC (0.59 eV), despite the symmetric appearance of the minimum-energy pathways resulting from the use of equivalent boundary configurations. The findings confirm that NbC offers more efficient and stable hydrogen trapping, making it superior for improving hydrogen tolerance in advance high-strength steels.

Original languageEnglish
JournalMetals and Materials International
DOIs
Publication statusAccepted/In press - 2026
Externally publishedYes

Keywords

  • First-principles calculation
  • Hydrogen embrittlement
  • NbC and VC precipitates
  • Press hardened steel
  • Trapping energy

Fingerprint

Dive into the research topics of 'Integrating Atomistic Simulations and Experimental Techniques to Unveil Hydrogen Trapping in Metal Carbide-Strengthened α-Fe'. Together they form a unique fingerprint.

Cite this