The development of silicone rubber materials with excellent thermal stability, flame retardancy and good mechanical properties remains a challenge. In this paper, an organosilicon crosslinker containing sulfur and nitrogen (S/N crosslinker) was designed and synthesized. A series of silicone rubbers with different crosslinkers were prepared by compounding tetraethyl orthosilicate (TEOS) with the S/N crosslinker in different proportions (10:0/7:3/5:5/3:7/0:10). Compared with TEOS-SR, the limiting oxygen index of the compound system increased to 28%-31%, and the peak heat release rate of 7:3-SR and 5:5-SR decreased by 32.3% and 38.4% respectively, while the char yield increased from 40% to 52%. In addition, the maximum decomposition peak temperatures of the compound system in nitrogen and air both shifted to higher temperatures. The tensile strength and elongation at break of 7:3-SR were 1.54 MPa and 388% respectively, which are significantly higher than those of TEOS-SR. The effects of the S/N crosslinker on the thermal stability, flame retardancy and mechanical properties of silicone rubber were systematically studied, and the “gas-phase/condensed-phase” synergistic flame retardant mechanism was revealed. This work provides a facile and effective molecular design strategy for the development of silicone rubber materials with high flame retardancy, high thermal stability and good mechanical properties.
| Original language | English |
|---|---|
| Article number | 112504 |
| Journal | Polymer Degradation and Stability |
| Volume | 254 |
| DOIs | |
| Publication status | Published - Dec 2026 |
| Externally published | Yes |
Keywords
- Flame retardancy
- S/N crosslinker
- Silicone rubber
- Thermal stability
Fingerprint
Dive into the research topics of 'Facile synthesis of a sulfur- and nitrogen-containing crosslinker and its flame retardant applications in silicone rubber'. Together they form a unique fingerprint.Cite this
- APA
- Author
- BIBTEX
- Harvard
- Standard
- RIS
- Vancouver