Free-standing nanoporous nickel (np-Ni) ribbons were directly synthesized by dealloying Mg90-xNixY10 metallic glass ribbons in citric acid aqueous solutions under free conditions. Due to the amorphous nature of the Mg90-xNixY10 precursors, the as-dealloyed samples exhibit a uniform nanoporous structure with the ligament size of ?7 nm. Effects of alloy composition, leaching time, and acid concentration on the resulting nanoporous microstructure were discussed. The lower limit of Ni content in Mg90-xNixY10 precursors was identified to be 20%, below which the nanoporous Ni could not be formed. Besides, a linear relationship was established between the ligament size and the leaching time on a logarithmic scale. The ultrafine structure of the obtained np-Ni was associated with the stabilizing effect of citric acid. The as-dealloyed samples with the naturally formed oxide surface of NiO were directly examined as binder-free electrodes for high-performance supercapacitors.
| Original language | English |
|---|---|
| Pages (from-to) | A348-A354 |
| Journal | Journal of the Electrochemical Society |
| Volume | 164 |
| Issue number | 2 |
| DOIs | |
| Publication status | Published - 2017 |
| Externally published | Yes |
UN SDGs
This output contributes to the following UN Sustainable Development Goals (SDGs)
-
SDG 7 Affordable and Clean Energy
Fingerprint
Dive into the research topics of 'Fabrication of three-dimensional nanoporous nickel by dealloying Mg-Ni-Y metallic glasses in citric acid solutions for high-performance energy storage'. Together they form a unique fingerprint.Cite this
- APA
- Author
- BIBTEX
- Harvard
- Standard
- RIS
- Vancouver