Enhancement of pitting corrosion resistance of austenitic stainless steel through deposition of amorphous/nanocrystalline oxy-nitrided phases by active screen plasma treatment

  • Yang Li*
  • , Yongyong He
  • , Jianxun Qiu
  • , Jun Zhao
  • , Qianwen Ye
  • , Yijie Zhu
  • , Junyuan Mao
  • *Corresponding author for this work
  • Yantai University
  • Tsinghua University

Research output: Contribution to journal › Article › peer-review

Abstract

In this research, AISI 304 austenitic stainless steels were efficient treatment using active screen plasma oxy-nitriding technique. The modified layers were characterized by X-ray photoelectron spectroscopy, X-ray diffraction, scanning electron microscopy, transmission electron microscopes, and atomic force microscopy. In addition, the pitting corrosion resistances of untreated and oxy-nitrided samples were analyzed by polarization method in 3.5 wt.% NaCl solution. The results showed that a duplex-layer consisting of a deposition layer and a diffusion layer (including CrN+α phase and nitrogen expanded austenite phase) was generated. Special concern has been given to the formation of an amorphous top layer for the deposition of nano sized oxy-nitrides. It believed that the deposition layer of oxy-nitrides formed on steel surface during active screen plasma oxy-nitriding that lead to improved corrosion resistance of AISI 304 austenitic stainless steel, so that the pitting corrosive attack can be avoided.

Original languageEnglish
Article numbere20170697
JournalMaterials Research
Volume21
Issue number6
DOIs
Publication statusPublished - Oct 2018
Externally publishedYes

Keywords

  • Austenitic stainless steel
  • Oxy-nitrided
  • Pitting corrosion
  • XPS