Abstract
(Nd1-xGdx)2(Ce 1-xZrx)2O7 (0 ≤ x ≤ 0.5) ceramic powders synthesised by the chemical-coprecipitation and calcination method were pressureless-sintered at 1,973 K for 10 h in air. The structure and electrical conductivity of (Nd1-xGdx) 2(Ce1-xZrx)2O7 ceramics were investigated by the X-ray diffraction and impedance spectroscopy measurements. (Nd1-xGdx)2(Ce 1-xZrx)2O7 (0 ≤ x ≤ 0.5) ceramics exhibit a single phase of defect fluorite-type structure. The electrical conductivity of (Nd1-xGdx) 2(Ce1-xZrx)2O 7 ceramics increases with temperature in the range 623-1,173 K following an Arrhenius law. At identical temperature levels, the measured electrical conductivity of (Nd1-xGdx) 2(Ce1-xZrx)2O 7 ceramics varies with doping different Gd2O3 and ZrO2 contents and exhibits a maximum at x = 0.1.
Original language | English |
---|---|
Pages (from-to) | 153-157 |
Number of pages | 5 |
Journal | Fuel Cells |
Volume | 11 |
Issue number | 2 |
DOIs | |
Publication status | Published - Apr 2011 |
Externally published | Yes |
Keywords
- (Nd Gd)(Ce Zr)O
- Ceramics
- Electrical Conductivity
- Impedance Spectroscopy