Abstract
3,4-Dinitrofurazanofuroxan (DNTF) is an indispensable carrier material for next-generation high-energy melt-cast explosives. Solidification performance dictates the fabrication scheme and final integrity of DNTF charges; nevertheless, the fundamental mechanism linking melt temperature to solidified microstructures remains poorly established. Herein, we systematically interrogate the undercooling response, nucleation-growth kinetics, morphological evolution, defect topology, and mechanical disparities of DNTF solidified from melts at distinct thermal states, with melt temperature identified as the central control variable. DSC measurements under low-disturbance conditions reveal that the 112 °C DNTF melt triggers nucleation at a mild undercooling of 16.1 °C with a crystallization onset temperature of 93.9 °C, whereas the 130 °C melt requires a drastically elevated undercooling of 73.1 °C, shifting the crystallization initiation point down to 36.9 °C. High-temperature melts undergo dominant heterogeneous nucleation at mold walls, yielding coarse radiating columnar dendrites and a tripartite casting architecture: fine surface equiaxed grains, central coarse columnar grains, and large central equiaxed grains. Such samples suffer from interconnected tunnel-like shrinkage cavities, delivering a casting density of 1.642 g/cm3 and a porosity of 15.2%. Conversely, abundant large molecular clusters in low-temperature melts furnish numerous viable nucleation sites and facilitate homogeneous nucleation. Concurrent equiaxed grain formation disrupts dendritic propagation, generating refined mixed microstructures devoid of prominent columnar domains, with discrete spherical microvoids as the prevailing defects; the casting density increases to 1.699 g/cm3 alongside a reduced porosity of 12.1%. Mechanical characterizations demonstrate that the interior regions of low-temperature castings achieve an average Vickers hardness of 19.6 (27.3% higher than high-temperature counterparts), an average compressive strength of 10.99 MPa (66.0% enhancement relative to 6.62 MPa for high-temperature specimens), and an average elastic modulus of 549.16 N/mm2 (32.1% increment). Such outstanding mechanical performance stems from the synergistic contributions of grain refinement strengthening, grain-boundary-mediated crack deflection and arrest, and spatially dispersed microdefects. This work elucidates the intrinsic cascade correlation "melt structure–solidification dynamics–microstructure-mechanical properties" for DNTF, offering critical theoretical insights and quantitative parametric references to guide the rational design and optimization of DNTF-based melt-cast charge forming workflows.
| Original language | English |
|---|---|
| Journal | Defence Technology |
| DOIs | |
| Publication status | Accepted/In press - 2026 |
| Externally published | Yes |
Keywords
- DNTF
- Mechanical properties
- Melt temperature
- Microstructure evolution
- Nucleation selection
Fingerprint
Dive into the research topics of 'Effects of melt temperature on solidification nucleation selection, microstructure evolution and mechanical properties of DNTF'. Together they form a unique fingerprint.Cite this
- APA
- Author
- BIBTEX
- Harvard
- Standard
- RIS
- Vancouver