Abstract
In this paper, Ti-6Al-4V alloy were successfully fabricated using a Spark Plasma Sintering (SPS), thermal deformation and heat treatment process. SPS sintering is divided into two steps: The first step is low-Temperature molding at 600°C and 300 MPa, and the second step is thermal deformation at 800°C, with a deformation of 70%. The effects of solution treatment and aging process at temperatures above and below the β transformation point on the microstructure and mechanical properties of Ti-6Al-4V are investigated. The study found that the mechanical properties were better after treatment (900°C, 30 min+ water quenching+550°C, 4 h).
| Original language | English |
|---|---|
| Article number | 012006 |
| Journal | Journal of Physics: Conference Series |
| Volume | 1855 |
| Issue number | 1 |
| DOIs | |
| Publication status | Published - 12 Apr 2021 |
| Event | 2020 International Symposium on New Materials and Technologies for Armor, ISMTA 2020 - Virtual, Online Duration: 25 Nov 2020 → 26 Nov 2020 |
Fingerprint
Dive into the research topics of 'Effects of heat-Treatment on microstructures and mechanical properties of hot deformed ti-6al-4v alloy'. Together they form a unique fingerprint.Cite this
- APA
- Author
- BIBTEX
- Harvard
- Standard
- RIS
- Vancouver