Compressive strength and failure mechanism of chemical vapor deposited zinc sulfide from room temperature to 600°C

Tianbao Cheng, Weiguo Li*, Rubing Zhang, Daining Fang

*Corresponding author for this work

Research output: Contribution to journalArticlepeer-review

2 Citations (Scopus)

Abstract

The compressive strength is a key factor for the design, application, and evaluation of the chemical vapor deposited (CVD) zinc sulfide (ZnS) in infrared optical engineering. However, to date, only the values of the compressive strength at room temperature (RT) have been reported. In this paper, the compressive strength of CVD ZnS from RT to 600°C is measured on the developed apparatus for high-Temperature mechanical testing. The failure mechanism in this temperature range is analyzed from both macro-And micro-scale. The study shows that the compressive strength of CVD ZnS from RT to 600°C has relatively large dispersion and weak temperature dependence. During compression, the specimen is crushed and the major fragments are slender columns which are almost as long as the specimen and have sides nearly parallel to the compression direction. The failure of the CVD ZnS is attributed to shear failure. Once shear slip occurs, the part below the slip plane is split to slender columns.

Original languageEnglish
Pages (from-to)133-140
Number of pages8
JournalHigh Temperatures - High Pressures
Volume46
Issue number2
Publication statusPublished - 2017
Externally publishedYes

Keywords

  • Chemical vapor deposition
  • Compressive strength
  • Failure mechanism
  • High temperature
  • Macro-And micro-scale
  • Zinc sulfide