Abstract
Designing elastomers that combine high mechanical strength with a broad damping-temperature range remains a major challenge for vibration attenuation and impact protection. Here, flexible 2, 4-pentanedione dioxime (2,4-PD) and rigid 2, 6-diaminopyridine (2,6-DAP) were used as complementary chain extenders to regulate the aggregation structure of poly(oxime-urethane-urea) (POUU) elastomers. The optimized POUU-P0.4D0.6 features local short-range order and long-range weak microphase separation. This hierarchical structure affords a tensile strength of 52.33 MPa, an elongation at break of 920.20%, and an effective damping-temperature range of 122.84 ℃ (12.9–135.7 ℃, tan δ ≥ 0.3). Temperature-dependent structural and spectroscopic results, together with calculated interaction energies, associate the broad damping response with sequential soft-segment relaxation, interfacial friction, and reorganization of locally associated domains. Repeated temperature scans, rate-dependent cyclic tensile tests, falling-ball measurements, and high-strain-rate compression further characterize the energy-dissipation and impact responses. These results establish a rigid-flexible molecular strategy for high-strength damping elastomers operating from room temperature to elevated temperatures.
| Original language | English |
|---|---|
| Article number | 182900 |
| Journal | Chemical Engineering Journal |
| Volume | 549 |
| DOIs | |
| Publication status | Published - 1 Dec 2026 |
| Externally published | Yes |
Keywords
- Broad damping-temperature range
- High strength
- Impact resistance
- POUU elastomer
- Rigid-flexible strategy
- Vibration attenuation
Fingerprint
Dive into the research topics of 'A rigid-flexible approach enables high-performance elastomers with broad damping temperature range and enhanced strength for vibration attenuation and impact resistance'. Together they form a unique fingerprint.Cite this
- APA
- Author
- BIBTEX
- Harvard
- Standard
- RIS
- Vancouver