Abstract
Morphological degradation at the Li/solid-state electrolyte (SSE) interface is a prevalent issue causing performance fading of all-solid-state batteries (ASSBs). To maintain the interfacial integrity, most ASSBs are operated under low current density with considerable stack pressure, which significantly limits their widespread usage. Herein, a novel 3D-micropatterned SSE (3D-SSE) that can stabilize the morphology of the Li/SSE interface even under relatively high current density and limited stack pressure is reported. Under the pressure of 1.0 MPa, the Li symmetric cell using a garnet-type 3D-SSE fabricated by laser machining shows a high critical current density of 0.7 mA cm–2 and stable cycling over 500 h under 0.5 mA cm–2. This excellent performance is attributed to the reduced local current density and amplified mechanical stress at the Li/3D-SSE interface. These two effects can benefit the flux balance between Li stripping and creep at the interface, thereby preventing interfacial degradation such as void formation and dendrite growth.
| Original language | English |
|---|---|
| Article number | 2104009 |
| Journal | Advanced Materials |
| Volume | 33 |
| Issue number | 49 |
| DOIs | |
| Publication status | Published - 9 Dec 2021 |
| Externally published | Yes |
Keywords
- 3D-micropatterned garnet
- all-solid-state batteries
- electrochemomechanics
- interfacial degradation
- solid-state electrolytes
- void formation
Fingerprint
Dive into the research topics of 'A Morphologically Stable Li/Electrolyte Interface for All-Solid-State Batteries Enabled by 3D-Micropatterned Garnet'. Together they form a unique fingerprint.Cite this
- APA
- Author
- BIBTEX
- Harvard
- Standard
- RIS
- Vancouver