Skip to main navigation Skip to search Skip to main content

A forming anisotropy CPFEM model of superalloys electroplasticity based on conductivity tensor

  • Rui Zhao*
  • , Changke Li
  • , Jiuxing Zhao
  • , Bao Meng
  • , Min Wan
  • *Corresponding author for this work
  • Beihang University

Research output: Contribution to journal › Article › peer-review

Abstract

Electro-assisted forming (EAF) was widely applied for forming thin-walled superalloy components. However, temperature, stress, dislocation, and Taylor factor are affected under different current loading directions and amplitudes, which remains insufficiently explained. This study conducted electrically assisted uniaxial tensile tests of superalloy GH4169 sheets. Based on EBSD observations, the current direction significantly influences the transition of grain boundaries from low angles to high angles, forming a unique deformation polarity. Then, a multi-grain RVE model considering the property difference of grain boundaries and interiors was established. Besides, an anisotropic electrical conductivity tensor and current direction factor were established. Based on this, a CPFEM (crystal plasticity finite element method) model was developed to describe the forming anisotropy. Furthermore, under various current directions and amplitudes, the evolution of temperature and dislocation density, as well as the variation of stress–strain curves and Taylor factor, were analyzed. This study provides a novel perspective for expanding the theoretical framework and an insightful interpretation of EAF applications.

Original languageEnglish
Article number116883
JournalMaterials and Design
Volume270
DOIs
Publication statusPublished - Oct 2026
Externally publishedYes

Keywords

  • CPFEM model
  • Electroplasticity
  • Forming anisotropy
  • Superalloys

Fingerprint

Dive into the research topics of 'A forming anisotropy CPFEM model of superalloys electroplasticity based on conductivity tensor'. Together they form a unique fingerprint.

Cite this