TY - JOUR
T1 - Investigation on the thermal decomposition of hydroxyl terminated polyether based polyurethanes with inert and energetic plasticizers by DSC-TG-MS-FTIR
AU - Ou, Yapeng
AU - Sun, Yalun
AU - Guo, Xueyong
AU - Jiao, Qingjie
N1 - Publisher Copyright:
© 2018 Elsevier B.V.
PY - 2018/6
Y1 - 2018/6
N2 - Thermal decomposition behavior of hydroxyl terminated polyether (HTPE) based polyurethanes (PUs) containing glycerol triacetate (TA), bis(2,2-dinitropropyl)-acetal/formal (BDNPA/F, also known as A3) and N-butyl-N-(2-nitroxyethyl)nitramine (NENA) respectively as plasticizers were investigated by the combination of differential scanning calorimetry-thermogravimetry-mass spectrometry-Fourier transform infrared spectroscopy (DSC-TG-MS-FTIR) techniques. Instead of DSC, DTG curves were applied to evaluate the compatibility since no intense exothermic effect appears in decomposition of HTPE based PU. Three plasticizers, especially the inert TA, were absolutely compatible with HTPE in perspective of engineering application according to the evaluated standard of compatibility. Decomposition of HTPE based PU after endothermic melting is a two-step process including, exothermic depolymerization succeed by intense decomposition. Influence mechanisms of energetic and inert plasticizers on decomposition of HTPE based PU are different. NO· free radical generated by the pyrolysis of NENA and A3 is the major incentive of chain scission resulting in depolymerization of HTPE based PU, and chain scission temperature are shifted forward with the increasing concentration of NO· as the NENA-PU is more vulnerable. While carbanion and electrophile intermediate resembling CO2 generated by decarboxylation reaction of carboxylic acid are the major reactive products in TA. Furthermore, micro defect caused by migration of TA in TA-PU accelerates the degradation of HTPE based PU under acidic condition.
AB - Thermal decomposition behavior of hydroxyl terminated polyether (HTPE) based polyurethanes (PUs) containing glycerol triacetate (TA), bis(2,2-dinitropropyl)-acetal/formal (BDNPA/F, also known as A3) and N-butyl-N-(2-nitroxyethyl)nitramine (NENA) respectively as plasticizers were investigated by the combination of differential scanning calorimetry-thermogravimetry-mass spectrometry-Fourier transform infrared spectroscopy (DSC-TG-MS-FTIR) techniques. Instead of DSC, DTG curves were applied to evaluate the compatibility since no intense exothermic effect appears in decomposition of HTPE based PU. Three plasticizers, especially the inert TA, were absolutely compatible with HTPE in perspective of engineering application according to the evaluated standard of compatibility. Decomposition of HTPE based PU after endothermic melting is a two-step process including, exothermic depolymerization succeed by intense decomposition. Influence mechanisms of energetic and inert plasticizers on decomposition of HTPE based PU are different. NO· free radical generated by the pyrolysis of NENA and A3 is the major incentive of chain scission resulting in depolymerization of HTPE based PU, and chain scission temperature are shifted forward with the increasing concentration of NO· as the NENA-PU is more vulnerable. While carbanion and electrophile intermediate resembling CO2 generated by decarboxylation reaction of carboxylic acid are the major reactive products in TA. Furthermore, micro defect caused by migration of TA in TA-PU accelerates the degradation of HTPE based PU under acidic condition.
KW - DSC-TG-MS-FTIR
KW - Energetic plasticizer
KW - Free radical oxidation
KW - HTPE
KW - Pyrolysis products
UR - http://www.scopus.com/inward/record.url?scp=85045197286&partnerID=8YFLogxK
U2 - 10.1016/j.jaap.2018.03.011
DO - 10.1016/j.jaap.2018.03.011
M3 - Article
AN - SCOPUS:85045197286
SN - 0165-2370
VL - 132
SP - 94
EP - 101
JO - Journal of Analytical and Applied Pyrolysis
JF - Journal of Analytical and Applied Pyrolysis
ER -